researchpp. 299–309

Influence of Heat and Mechanical Treatments on the Mechanical and Structural Characteristics of Molded Manganese Steels

This paper presents a study to improve the performance of Fe-Mn-C cast steels containing 1.7% and 2.7% Cr by weight, using two treatment methods (thermal and mechanical) applied separately to two different steel grades. This approach enables an extended service life for components such as crusher liners, mill hammers, and level crossings, without requiring complete recasting. The experimental techniques used for characterization included spark optical emission spectroscopy, optical microscopy, scanning electron microscopy, as well as micro- and macro-hardness testing. Steel 1, with a…

Keywords
carbides hardness heat treatment manganese steel mechanical treatment microstructure
10 Views1 Downloads0 Citations
researchpp. 310–331

Polyoxometalates as Catalysts for Biomass Conversion: Properties, Applications, and Regenerability

Polyoxometalates (POMs) have emerged as exceptionally versatile catalysts for green chemical reactions, demonstrating significant potential in the sustainable valorization of biomass. Their tunable Brønsted/Lewis acidity and redox properties enable a broad range of chemical transformations, offering remarkable flexibility in process design. This mini review provides a summary of recent advances in the thermocatalytic conversion of biomass using POMs, addressing their utilization as both homogeneous and heterogeneous catalysts. Key reaction pathways, including solvolysis, oxidation,…

Keywords
acid catalysis biomass catalytic process polyoxometalates redox catalysis
55 Views0 Downloads0 Citations
researchpp. 332–347

Design and Development of a Water Flow Monitoring Device using Mitsubishi FX3U-14MT PLC

Efficient water management is essential for ensuring sustainability and reducing operational costs, especially in small to medium-scale buildings such as schools, health clinics, and office facilities. This paper presents the design and implementation of a cost-effective automated water flow monitoring system, integrating a Mitsubishi FX3U-14MT PLC with an Arduino module to facilitate real-time flow measurement and precise control of solenoid valves. The PLC is programmed using ladder logic, while the Arduino is responsible for processing sensor data, thereby enhancing measurement accuracy…

Keywords
Arduino Mitsubishi FX3U-14MT PLC PLC solenoid valve water flow monitoring
7 Views0 Downloads0 Citations
researchpp. 348–365

Optimizing Evaporator Design in ORC Systems for Waste-to-Energy Conversion Using FAST Diagram and Value Engineering

The global waste crisis necessitates innovative solutions for sustainable energy conversion. This study presents a comprehensive optimization framework for evaporator design in Organic Rankine Cycle (ORC) systems utilized in waste-to-energy conversion. This research integrates the Function Analysis System Technique (FAST) diagram with Value Engineering (VE) principles to assess the logical hierarchy and cost analysis components of system effectiveness. Evaluation of the 887 kW shell-and-tube evaporator showed tubes, baffles, and shells account for 90% of production costs and are the most…

Keywords
energy efficiency evaporator optimization FAST diagram organic rankine cycle value engineering waste management
11 Views2 Downloads0 Citations
researchpp. 366–378

Enhanced Finite Element Numerical Analysis of Rigid Inclusion Lateral Resistance for Embankment on Slightly Overconsolidated Soft Clay

Soft clay soils represent a significant challenge for embankment construction due to high compressibility, low shear strength, low bearing capacity, and excessive settlement potential. This study presents an enhanced finite-element model to evaluate the performance of Mortar Column Inclusion (Inklusi Kolom Mortar, or IKM) as a rigid inclusion supporting embankments over slightly overconsolidated soft clays, as implemented in the Serang-Panimbang Toll Road Project (STA 75+600 to STA 75+800). The propose approach integrates depth-dependent multilinear lateral resistance with structural “dummy”…

Keywords
finite element numerical modeling ground improvement lateral resistance mortar column inclusion slightly overconsolidated clay
1 Views0 Downloads0 Citations
researchpp. 379–396

Improving Single-Phase Induction Motor Speed Control Using Model Reference Adaptive System and Fuzzy-Pid Regulator

As industries strive to enhance their applications to meet growing market demand, accurate speed control of single-phase induction motors (SPIMs) remains a crucial concern. This paper presents the modelling and simulation of SPIM speed control based on a hybrid Model Reference Adaptive System (MRAS) integrated with a Fuzzy–PID regulator. Superior performance was achieved by integrating MRAS with a fuzzy-PID regulator using an adaptive self-tuning mechanism. The purpose of this integration was to leverage the adaptive nature of MRAS and the robustness of the Fuzzy-PID regulator to enhance…

Keywords
fuzzy-PID model reference adaptive system (MRAS) sensorless SPIM speed control speed stability
2 Views0 Downloads0 Citations
researchpp. 397–416

An Enhanced Fuzzy Logic-Particle Swarm Optimization Algorithm for the Strategy Control of Self-driving Electric Vehicles

With the current rapid advancement of science and technology, there is an increasing focus on comprehensive research and the development of practical solutions for self-driving electric cars to address challenges, including environmental pollution, renewable energy utilization, emission control, and battery recycling. In this study, automatic direction control is achieved for electric vehicles by implementing line-tracing autonomous vehicles equipped with computer vision-based cameras, utilizing Particle Swarm Optimization (PSO), the Takagi–Sugeno Fuzzy model, and the PID control system.…

Keywords
autonomous vehicles camera fuzzy line tracking fuzzy-pso controller line tracking self-driving
11 Views0 Downloads0 Citations

No articles match the selected filter or search query.

Call for Papers

Submit Your Manuscript for the Next Issue

Contribute original research, review articles, and scholarly perspectives for our upcoming issue. Manuscripts will be handled through a structured editorial screening and peer-review workflow.

Call for Papers is open
Peer Reviewed DOI Assigned Open Access Indexing Ready