This paper deals with one-dimensional dynamic modelling and simulation of deep -bed com drying by two-phase model or heterogeneous model The models consider mass and heat transfer process within grain and drying air phase. This model also considers moisture content and temperature gradient within grain. The coupled of partial differential equations developed, then solves numerically by finite difference with altemating direction implicit method algorithm. The dynamic models predict not only humidity and temperature of outlet drying air, but also grain moisture content and temperature. The…

DOI
Keywords
0 Views0 Downloads0 Citations
Article

Kaji Eksperimental Dan Numerik Tentan G Faktor Ketangguhan Retak Modus I Dan Ii Pada Laminate Karbon/epoxy Serat Teranyam

This paper presents experimental and numerical analysis on the influence of crack orientations to the fracture toughness of mode I and mode II for woven type carbon/epoxy four ply laminate. The experimental procedure is carried out through off axis tensile test (ASTM D 3039-76) with nine variation of crack orientations i.e. 5°, 10°, 15°, 30°, 45° 65°, 75°, 80°, and 90°. Three rail shear test (ASTM D 4255-83) is utilized for zero degree crack orientation. The stress and strain contours around crack tips are obtained numerically using the finite element method. Numerical and experimental…

DOI
Keywords
0 Views0 Downloads0 Citations
Article

Kaji Eksperimental Pengaruh Waktu Penahanan Cair Terhadap Pembentukan Grafit Bulat Pada Proses Pengecoran Besi Cor Nodular 700

Nodular graphite on iron casting can be formed because of the present of Mg element from 0.02% - 0.05%, which is alloyed with iron base material to form FeSiMg through inoculation effect. At the pouring stage, especially in continuous production, Mg in the melting fluid and its inoculation effect decrease so that the formed graphite will not round as expected and certainly weaken its mechanical properties.This writing discuss the maximum holding time for the melting fluid in a ladle to assure acceptable mechanical properties, through experimental analysis of roundness of nodular graphite…

DOI
Keywords
0 Views0 Downloads0 Citations
Article

Fracture Behavior of Acrylonitrile-butadiene-styrene Resin

In this research, mixed mode loading testing of actylonitrile-butadiene-styrene (ABS) resin was carried out by using a compact tension shear specimen which was attached to a special loading device. The angle between the loading axis and the crack surface was varied from 90o (Mode I) to 0° (Mode I1). Two types of ABS resin were examined. The first one (ABS-I) has a butadiene rubber content of 18 wt % in the form of small particles of diameter about 200 nm. The second one (ABS-2) has the same overall butadiene rubber content but a bimodal particle distribution with diameters of 200 nm and 500…