researchpp. 121–121

Bonding at Particle Contacts

. This investigation deals with the behavior of cohesive bonding at particle contacts in soil. Direct measurement of cohesive strength at sliding contacts between particles of soil has not been accomplished. An indirect method is used in this study to estimate average contact cohesion from measurement of total strength of soil specimens. Two types of materials were tested; Ottawa sand and crushed quartz, with two different relative densities, 25 and 75 percents; each material was tested with four different cement contents, 0, 2, 4, and 6 percents of cement by weight. Adding cement was to…

Keywords
Cohesive bonding Particle contacts Sliding contacts Contact cohesion
0 Views0 Downloads0 Citations
researchpp. 133–133

Studi Eksperimental terhadap Parameter Daktilitas Struktur Baja

Abstrak. Makalah ini menyajikan studi eksperimental terhadap daktilitas struktur baja berupa portal sederhana dengan tujuan meneliti parameter-parameter yang berpengaruh terhadap daktilitas struktur baja, dan melakukan validasi terhadap usulan formula daktilitas struktur yang sedang dikembangkan melalui studi numerik. Sebelum dilakukan pengujian di Laboratorium terlebih dahulu dilakukan penelusuran teori-teori serta data-data dari hasil-hasil penelitian sebelumnya. Selanjutnya dilakukan simulasi komputer dengan menggunakan paket program analisis nonlinier MSC/NASTRAN untuk mengetahui…

Keywords
Daktilitas struktur Parameter daktilitas Formula daktilitas Validasi formula daktilitas
0 Views0 Downloads1 Citations
researchpp. 145–145

Analisis Kolom Langsing Beton Mutu Tinggi Terkekang terhadap Beban Aksial Tekan Eksentris

Abstrak. Studi ini bertujuan untuk mengetahui perilaku mekanik dari kolom langsing beton mutu tinggi terkekang yaitu beban kritis, lendutan di tengah kolom, daktilitas perpindahan, serta faktor pembesaran momen. Untuk menentukan faktor-faktor di atas maka dilakukan proses analisis yang dikenal dengan analisis P-Δ atau analisis orde kedua dengan memperhitungkan efek stabilitas kolom. Analisis menggunakan penampang kolom langsing beton bertulang mutu tinggi terkekang dengan metoda numerik. Kolom langsing dibebani oleh kombinasi beban aksial tekan dan momen lentur. Variabel yang digunakan…

Keywords
Kolom langsing Nilai kelangsingan Beton mutu tinggi terkekang Beban kritis Mekanisme keruntuhan Lendutan Daktilitas perpindahan Faktor pembesaran momen
0 Views0 Downloads2 Citations
researchpp. 155–155

Modulus Kekakuan Campuran Beraspal yang Mengandung Butiran Ban Bekas Sebagai Agregat Pengganti Sebagian

Abstrak. Selama dua dekade terakhir, metoda untuk perencanaan perkerasan lentur dikembangkan berdasarkan metoda analitik, dimana dalam pemakaian metoda ini sangat diperlukan untuk mengetahui modulus kekakuan dari material perkerasan. Tujuan utama dari penelitian yang diuraikan dalam tesis ini adalah untuk menentukan dan membandingkan nilai modulus kekakuan dari campuran beraspal yang mengandung butiran ban bekas sebagai agregat pengganti sebagian dengan campuran beraspal Konvensional. Campuran Hot Rolled Asphalt (HRA) tipe C (BS594.1992) dipilih dalam penelitian ini, dan pengaruh butiran ban…

Keywords
Modulus Butiran ban bekas HRA Agregat pengganti
0 Views0 Downloads2 Citations