DECREASING THE HARDNESS Ca, Mg AND HEAVY METALS Fe, Mn, Zn IN RAW WATER WITH ZEOLITE FROM CIKALONG, TASIKMALAYA
The decrease of hardness (Ca, Mg) and heavy metal (Fe, Mn, Zn) contents in raw water was conducted by flowing the sample water through the activated zeolite bed column. Treated water obtained from the experiment obviously met the parameter ……