Current Issue

Journal of Mathematical and Fundamental Sciences Vol. 43 Issue 1 2011

Vol. 43 No. 1 (2011)

Issue Articles

Articles Published in This Issue

Explore peer-reviewed research articles published in this issue.

researchpp. 1–8

Locating-Chromatic Number of Amalgamation of Stars

Let G be a connected graph and c a proper coloring of G. For i Æ’­1,2,Æ’»,k define the color class i C as the set of vertices receiving color i. The color code c (v) "ž¨ of a vertex v in G is the ordered k -tuple 1 ( (, ),, (, )) k d v C Æ’» d v C where (, ) i d v C is the distance of v to i C. If all distinct vertices of G have distinct color codes, then c is called a locating-coloring of G. The locating-chromatic number of graph G, denoted by ( ) L ƒÓ G is the smallest k such that G has a locating coloring with k colors. In this paper we discuss the locating-chromatic number of…

0 Views0 Downloads0 Citations
researchpp. 19–42

On Tight Euclidean 6-Designs: An Experimental Result

A finite set n X ⊆ ℝn with a weight function w: X → ℝ > 0 is called Euclidean t-design in ℝ > 0 (supported by p concentric spheres) if the following condition holds:           1 i p i i i S x X w X f d w f S      x x  x x for any polynomial f(x) ∈ Polℝ > 0 of degree at most t. Here Si ℝn is a sphere of radius ri ≥ 0, Xi=X ∩ S, and σi(x) is an O(n) -invariant measure on Si such that |Si|=rin-1|Sn-1>|, with |Si| is the surface area of Si and |Sn-1|is a surface area of the unit sphere in ℝn. Recently, Bajnok [1]…

0 Views0 Downloads0 Citations
researchpp. 43–50

Demethylation of Quinine Using Anhydrous Aluminium Trichloride

Quinine is a natural alkaloid having a methoxy group bound to quinoline ring and an allyl group bound to quinuclidine ring. Demethylation of quinine applying strong acid such as HBr or HI at high temperature was unsuccessful. The aim of this research was to obtain demethylated quinine by means of mild and selective demethylation procedure to prevent the addition reaction of allyl group. Selective demethylation of quinine has been carried out using anhydrous aluminium trichloride as reagent. The demethylation product was achieved in 68.12% yield by mole ratio of quinine to anhydrous aluminium…

0 Views0 Downloads0 Citations
researchpp. 59–72

Hierarchically Porous ZSM-5 Synthesized by Nonionic- and Cationic-Templating Routes and Their Catalytic Activity in Liquid-Phase Esterification

Hierarchically porous MFI zeolites (ZSM-5) have been synthesized by hydrothermal treatment in the presence of trialkoxysilylated-derivatives of nonionic poly(oxyethylene) alkyl ether or alkyl quaternary ammonium cation as mesopore-generating agent, along with tetrapropylammonium cation as zeolite structure-directing agent. Powder X-ray diffraction revealed that zeolites have been crystallized, and scanning electron microscopy showed rugged surface morphology that was quite different from conventional ZSM-5. The mesoporosity was confirmed by nitrogen adsorption-desorption measurement showing…

0 Views0 Downloads0 Citations
researchpp. 9–18

Doping Calcia and Yttria into Zirconia Obtained from by Product of Tin Concentrator to Improve its Ionic Conductivity

Zirconia has been prepared from Zircon concentrate by caustic fusion methods. Zircon is a by product from tin ore concentration plant at Bangka island of Indonesia. Yttria Stabilized-Zirconia (YSZ) was prepared by introducing the 8 % mol yttrium oxide into zirconia and sintered at 1500 "žaC for 5 hours. In order to obtain constant oxygen vacancy of 8 % mol in Zirconia, an appropriate amount of Yttria and Calcia were introduced into Zirconia and the mixtures were heated at 1350 oC for 5 hours. Elemental composition was determined by SEM/EDX and XRF and lattice parameters were determined using…