researchpp. 1–1

Experimental Investigation on the Effect of Web Opening Dimension on the Behavior of R/C Hybrid Deep T-Beam Subjected to Pure Torsion

. An experimental study was conducted to investigate the effect of web opening dimension on the behavior of reinforced concrete hybrid deep T-beam subjected to pure torsion. Four reinforced concrete hybrid deep T-beams were tested under pure torsion, where the three beams with different dimension of circular web opening and the other beam without opening as a reference beam. The testing program and experimental results are presented. The results show that dimension of circular web opening with diameter more than 100 mm significantly reduces the cracking and ultimate torque. It is also shown…

Keywords
Reinforced concrete hybrid deep T-beams Web opening dimension Crack pattern Cracking torque Ultimate torque Angle of twist
0 Views0 Downloads2 Citations
researchpp. 19–19

Pengaruh Beban Berulang terhadap Lebar Retak Pelat Beton Satu Arah dengan Pendekatan Mekanika Retakan

Abstrak. Masalah lebar retak merupakan hal yang masih memerlukan penelitian lebih lanjut. Rumusan yang ada masih menunjukkan penyebaran yang lebar dan pengaruh beban berulang terhadap lebar retak dianggap belum memuaskan. Hal ini telah diungkapkan oleh beberapa peraturan internasional seperti Eurocode 2 dan ACI 318. Analisis tentang pengaruh beban berulang terhadap lebar retak pelat beton satu arah dengan pendekatan mekanika retakan akan mengamati pengaruh variasi tegangan baja, angka tulangan, dan beban berulang. Analisis tinggi retak awal (ξi ) dan laju perambatan retak (ξi = f(fs,N))…

Keywords
Beban berulang Laju perambatan retak Lebar retak
0 Views0 Downloads0 Citations
researchpp. 35–35

Simulasi Dampak Peningkatan Demand terhadap Energi Listrik dalam Pemodelan Pengoperasian Waduk Kaskade

Abstrak. Peningkatan kebutuhan (demand) terutama air baku non irigasi pada dewasa ini relatif tidak dapat terkendali secara sistemik dalam kerangka tata ruang. Hal ini antara lain disebabkan oleh pertumbuhan kegiatan ekonomi yang mendorong arus urbanisasi yang sangat cepat dan terpusat pada suatu wilayah tertentu. Daerah Aliran Sungai (DAS) yang merupakan wilayah hidrologis yang mendukung keberlanjutan sumber air relatif tetap dan bahkan berkurang dari waktu ke waktu akibat pengembangan DAS yang tidak berwawasan lingkungan. Oleh karena itu, dalam rangka pemanfaatan sumber air secara optimal…

Keywords
Pengoperasian waduk kaskade Model optimasi programa non linier Simulasi trade off
0 Views0 Downloads2 Citations
researchpp. 9–9

Simulasi Perhitungan Tebal Selimut Beton Minimum terhadap Perubahan Jarak Bangunan dari Garis Pantai

Abstrak. Masalah serangan dari klorida biasanya muncul ketika ion klorida dari luar masuk ke beton. Pada umumnya, sumber dari ion klorida adalah air laut yang bersetuhan dengan beton. Tetapi, klorida juga dapat berada di permukaan beton dalam bentuk tetesan uap air laut yang sangat halus (berasal dari penguapan yang terjadi di laut dan dibawa oleh angin) atau dalam bentuk debu yang kemudian menjadi basah karena embun. Klorida dalam bentuk itu dapat terbang sampai lebih 2km dari garis pantai. Karena itu, studi analisis ini bertujuan untuk mengetahui tebal selimut beton dan W/C yang optimal…

Keywords
Tebal selimut beton Ion klorida Korosi Kerusakan beton