The Use of Waste Plastic as a Partial Substitution Aggregate in Asphalt Concrete Pavement
. As a developing country, Indonesia faces serious problems managing solid waste such as plastic. Annually, Indonesia produces approximately 5.4 million tons of waste plastic, accounting for 14% of the country